Proceedings Papers

... of total sulfide to total iron was 5.24. Calculated SI values of FeS using ScaleSoftPitzerTM 2019 software developed by Rice University were 2.2 at pH 6.7 and 0.8 at pH 5.2. The SI value of Barite was 2.0 at both pHs. FeS scale inhibition and dissolution Abstract Sulfide scales...
Proceedings Papers

...In the geological field, since carbonates are very commonly found as minerals, extensive studies have been made to understand the mechanism of dissolution 5 - 9 . Dissolution kinetics of iron carbonate was studied for a range of temperatures and pressures 10 - 16 . The effects...
Proceedings Papers

... areas of study. elemental sulfur chemical physical sulfur solvent precipitation deposition dissolve dissolution amine polysulfide hydrocarbon hydrogen polysulfide corrosion inhibition INTRODUCTION Mitigating elemental sulfur deposition and managing the associated sulfur-accelerated...
Proceedings Papers

...In the present work we have investigated the growth and dissolution of calcium carbonate in the presence of various additives, involving groups which may be ionized in aqueous solutions and have therefore the potential of interaction with solid surfaces. Both in crystal growth and dissolution...
Proceedings Papers

...Abstract Combination of a constant composition (CC) crystallization approach together with atomic force microscopy (AFM) has enabled the elucidation of the mechanisms of the scale (crystals) formation and dissolution at the molecular level. The new model reveals that the surfaces may be unable...
Proceedings Papers

... have studied on the corrosion behavior of alloy 625 and its constituent metals (Ni, Cr and Mo) in 0.05mol/kg HCl + 0.48mol/kg O2 at 350°C and 24MPa. They found that pure Ni suffers from severe general corrosion, and pure Cr and Mo undergo transpassive dissolution 9 . Aki et...
Proceedings Papers

... specimens measured after the removal of oxide films provides the net weight loss of the metal, ΔWFe,net, which corresponds to the total weight of the metal consumed by corrosion including oxidation and dissolution. Figure 3 shows the changes in ΔWFe,net...
Proceedings Papers

... initiation and propagation fracture surfaces. The initiation surfaces show evidence of dissolution, and propagation surfaces exhibit characteristics of microcleavage. Different fundamental mechanisms probably operate during these two stages. In the past, the bulk of the research effort has been devoted...
Proceedings Papers

..., but these factors were not investigated in this report. The dissolving ability is not analogous to acid dissolution of CaCO3 and therefore this chemical dissolver has more specialized applications. Several case histories of successful applications of this chemical dissolver are presented. Related...
Proceedings Papers

... currents, whereas segregation at grain boundaries prompts intergranular attack. Analytical electron microscopy measurements reveal silicon enrichment and chromium depletion at internal interfaces in irradiated specimens. Silicon enhances dissolution at transpassive potentials, whereas chromium depletion...