Abstract
Flow accelerated corrosion, corrosion fatigue, and stress corrosion are the three most common failure mechanisms for HRSG boiler tubes and components. The causes of these failure mechanisms in HRSGs are discussed and examples of each mechanism provided. Challenges associated with predicting high risk locations for inspection are discussed. Guidance is available to diagnose these failure mechanisms in the field. Areas of research needed to assist designers, operators, and maintenance staff in predicting and preventing failures are also identified.
© 2003 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).
2003
Association for Materials Protection and Performance (AMPP)
You do not currently have access to this content.