Abstract
Eight-year atmospheric corrosion tests of A 588B weathering steel were conducted in industrial, marine, and rural environments. The material was tested following two types of heat treatment: (1) quenched-and-tempered to produce a tempered martensite microstructure, and (2) normalized to produce a microstructure comprised of ferrite and pearlite. The results of these tests indicate that these heat treatments have no effect on the corrosion resistance, and that the performance of weathering steels can be estimated solely on the basis of composition.
© 2000 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).
2000
Association for Materials Protection and Performance (AMPP)
You do not currently have access to this content.