Chloride contamination of amines in contact with stainless steel creates a well known potential for stress corrosion cracking (SCC). A far less recognized hazard of chloride contamination, when sulfides are present, is drastically accelerated generalized corrosion. Chloride induced corrosion can be avoided with an inlet gas reverse flow coalescer and an inlet slug catcher to knock out brine bearing oroduced water. If the amine is already contaminated with chlorides, steps can be taken to minimize this type of corrosion such as better amine filtration, amine reclamation, and using stainless steel with higher nickel contents.
© 1997 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).
1997
Association for Materials Protection and Performance (AMPP)
You do not currently have access to this content.