Causes of poor reverse osmosis (RO) performance and/or failure include scale formation, iron deposition, and biological fouling. Benchtop and field tests were used to screen products for their activity against these foulants. Experimental techniques and results are discussed.
© 1993 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).