Combustion environments generated by incineration of household garbage (municipal wastes) as well as industrial wastes are described. Principal corrosion modes in various incinerators are discussed. The corrosion behavior of various alloys in incinerators is presented. The paper focuses on a new commercial alloy based on the Ni-Co-Cr-Si system and its performance capability in various incinerators.
© 1991 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).