Abstract
This paper summarizes the work accomplished by the NACE TASK GROUP on DEAERATOR CRACKING, T-7H-7. Included are statistics relevant to industry segment on the incidence and severity of deaerator cracking. Guidelines are summarized and failure analysis case studies discussed. Operation and water chemistry parameters that potentially accelerate the environmentally assisted corrosion process best described as corrosion fatigue will be listed and discussed.
© 1988 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).
1988
Association for Materials Protection and Performance (AMPP)
You do not currently have access to this content.