Various corrosion inhibitors were evaluated in a dynamic corrosion test loop which is equipped with deposit and corrosion monitors and with pH and blowdown controllers. The Auger depth profiles were used to study the compositions and thicknesses of films formed by these corrosion inhibitors as a function of pH.
© 1988 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).