Abstract
Avesta 254SMO (UNS S31254) has been extensively applied in paper mill bleach plants in Scandinavia. A review of twenty installations in operating mills indicates that S31254 has performed well as a remedy to corrosion problems of 316L, 317L, and 904L. S31254 is now regularly used in the construction of major bleach plant components. Corrosion performance has been good for periods now extending beyond eight years.
Subject
Materials,
Piping,
Pulp,
Nozzles,
Rolling,
Filters,
Repair,
Crevice corrosion,
Linings,
Towers,
Pitting,
Construction,
Stainless steel
© 1987 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).
1987
Association for Materials Protection and Performance (AMPP)
You do not currently have access to this content.