Abstract
The results of a planned interval test of 90 days duration in a model flue gas desulfurization system are discussed. Tests were conducted in a high chloride, limestone slurry based environment containing fluoride and flyash. Corrosion in absorber and outlet duct zones is outlined in terms of relative tendencies of localized corrosion propagation for six alloys.
© 1986 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).