This paper presents the results of an investigation of the erosion-corrosion behaviour of copper-nickel alloys (90:10 Cu/Ni and 7030 Cu/Ni), nickel-copper alloy UNS N04400 and nickel-based alloys (UNS N06022, N06030 and UNS S32550) used as heat exchanger tubes, in warm flowing Arabian Gulf seawater containing up to 5 ppm of sulphide ions. Visual and optical examinations of the internal surfaces of the tubes were carried out to compare the susceptibilities to erosion-corrosion attack of the different alloys, taking into consideration the nature of the product films formed.
© 1994 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).
1994
Association for Materials Protection and Performance (AMPP)
You do not currently have access to this content.