Abstract
Test racks containing creviced, welded coupons of stainless steels, nickel base alloys and titanium have been exposed in various parts of the gas cleaning systems in three municipal waste incineration plants. The flue gases were rich in hydrogen halides and the environments in the cleaning systems were very corrosive causing mainly crevice and pitting corrosion. The best corrosion resistance was shown by the superaustenitic stainless steel S32654 and the nickel base alloys N10276 and N06022. Titanium performed badly and was attacked by excessive uniform corrosion.
© 1994 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).
1994
Association for Materials Protection and Performance (AMPP)
You do not currently have access to this content.