After a seven month exposure period, the control and polarized samples were taken out of the intake canal and tested for corrosion, microbiological fouling and surface chemistry. Deposits and corrosion products were further tested using EDX and Auger analyses. A correlation between the sample polarization and the results of different surface analyses is presented.
© 1992 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).