Abstract
Intergranular stress corrosion cracking may occur in the weld-heat-affected zone of susceptible stainless steel materials which have been used in some boiling water reactor piping systems. One of the prerequisite conditions for stress corrosion attack is a high tensile stress in the exposed, locally sensitized material near the weld root. Several processes have been developed which can deter stress corrosion attack by altering the residual stress distributions near the welds to ensure that low stresses prevail in critical locations. These residual stress modification remedies and their qualification testing are described in this paper.
© 1983 Association for Materials Protection and Performance (AMPP). All rights reserved. No part of this publication may be reproduced, stored in a retrieval system, or transmitted, in any form or by any means (electronic, mechanical, photocopying, recording, or otherwise) without the prior written permission of AMPP. Positions and opinions advanced in this work are those of the author(s) and not necessarily those of AMPP. Responsibility for the content of the work lies solely with the author(s).
1983
Association for Materials Protection and Performance (AMPP)
You do not currently have access to this content.