CORROSION SCIENCE
Initial Stages of the Anodic Oxidation of Iron in Chloride Solutions
CORROSION (1991) 47 (12): 908–916.
Fracture Mechanics Data and Modeling of Environmental Cracking of Nickel-Base Alloys in High-Temperature Water
CORROSION (1991) 47 (12): 917–938.
Deformation Effects on Intragranular Carbide Precipitation and Transgranular Chromium Depletion in Type 316 Stainless Steels
CORROSION (1991) 47 (12): 939–947.
Technical Note: Distribution of Initial Current Between Bare and Filmed Surfaces: What Is Being Measured in a Scratched Electrode Test?
CORROSION (1991) 47 (12): 948–951.
Determination of Coating Deterioration with EIS: I. Basic Relationships
CORROSION (1991) 47 (12): 958–963.
Discussion on the Relationship of Break-Point Frequencies to Delamination
CORROSION (1991) 47 (12): 964–965.
CORROSION ENGINEERING
Predictive Model for CO2 Corrosion Engineering in Wet Natural Gas Pipelines✫
CORROSION (1991) 47 (12): 976–985.