The marine immersion corrosion of irons and steel under calcareous deposition (principally calcium carbonate) is known to be relatively low for shorter exposures (e.g., a few years). Herein the effect of calcareous deposition on corrosion is considered for exposures up to 1,300 y. The data are derived from archaeological steel and iron shipwrecks, cast iron cannons and cannonballs, and wrought iron anchors in locations where there was direct evidence, in and on the corrosion products, of calcareous deposition. Such deposition promotes formation of calcium and ferrous carbonate layers of low permeability on and within rusts. These tend to inhibit both early and long-term corrosion rates. The data show that up to about 200 y exposure corrosion losses as a function of time can be approximated closely by a linear function of time. Longer exposures follow a moderate power-law function, consistent with diffusion considerations. Comments are made about the likely interplay between calcareous deposition and microbiological corrosion.
Skip Nav Destination
Article navigation
1 May 2021
Research Article|
February 16 2021
Long-Term Immersion Corrosion of Irons and Steel in Seawaters with Calcareous Deposition
R.E. Melchers
R.E. Melchers
‡
Centre for Infrastructure Performance and Reliability, The University of Newcastle, Callaghan, Australia.
‡Corresponding author. E-mail: [email protected].
Search for other works by this author on:
‡Corresponding author. E-mail: [email protected].
Online ISSN: 1938-159X
Print ISSN: 0010-9312
© 2021, NACE International
2021
CORROSION (2021) 77 (5): 526–539.