Iron alloys containing titanium oxidized in air at 1000C (1832 F) at a rate diminishing as titanium content increased. Relative thicknesses of three oxide layers were markedly different from thicknesses measured on pure iron exposed under like conditions.
© 1967 National Association of Corrosion Engineers
1967